Products

Home > ProductsThe PbSnTe-based thermoelectric ingot for thermoelectric power generation modules,good for converting 500-800K heat sources into electricity

The PbSnTe-based thermoelectric ingot is grown by the Thermonamic with the alloy of Pb, Te, Sn and others, and our unique crystallizing processes. The Lead Telluride thermoelectric ingot is used to fabricate the modules for power generation, good for converting 500 ~ 800 K heat sources into electricity. The peak of dimensionless figure of merit (ZT) of our P-type and N-type ingots is larger than 0.9 and 1.1 around 700 K respectively, making them good for waste heat recovery. Meanwhile, our ingot is featured with good mechanical strength and highly stable property, providing the key elements for producing the high performance and reliable power generation modules used for middle temperature range heat sources.

 

Performance Specification

p-Type

n-Type

Note

Part Number

TIG-PbTe-P-1

TIG-PbTe-N-1

Diameter (mm)

22 ± 0.5

22 ± 0.5

Length (mm)

61 ± 5

61 ± 5

Electrical Conductivity (σ / 102 S m-1)

900 ~ 1200

1900 ~ 2300

300 K

Seebeck Coefficient (α / μV K-1)

100 ~ 180

100~ 210

350 ~ 800K

Thermal Conductivity (κ / W m-1 K-1)

1.1 ~ 2

1.7 ~ 3

300 ~ 800k

Power Factor ( P / W m K-2)

≥ 0.0018

≥ 0.003

700 K

ZT value

≥ 0.9

≥ 1.2

700K